Due to the Middle East situation, the Strait of Hormuz is lockdown. The raw materials are very short, so C5 hydrocarbon resin and C9 hydrocarbon resin prices went up substantially. All the offers a...
2026-03-13
The reasons why thermoplastic road marking paint becomes dark:1. Heating temperature is too high, the coating is burnt. The normal heating termperature is 180-210℃.2. The mixing is not well-distr...
2021-07-09
There are some customers mentioned the problem of falling off during the construction of thermoplastic road marking pain...
2020-07-28
1.Resin’s softening point is lower. Reason: At present, thermoplastic road marking paint factories pursue better fluid...
2020-07-28
Characteristic difference: C5 hydrocarbonresin has little odor and high adhesion。C9 hydrocarbon resin has strong odor an...
2020-07-14
C5 hydrocarbon resin is widely used for thermoplastic road marking paint due to its competitive price and good performan...
2020-07-14
|